Sook-Hwan Kim 5 Articles
Microstructures and Mechanical Properties of the Friction Stir Welded Dissimilar Joint of AZ31B/A6061
Heung-Ju Kim, Chang-Keun Cheon, Sook-Hwan Kim, Woong-Seong Chang
J Weld Join. 2006;24(4):6-10.   Published online October 16, 2006
PDFPDF    
Lower Temperature Soldering of Capacitor Using Sn-Bi Coated Sn-3.5%Ag Solder
Mi-Jin Kim, Sun-Yun Cho, Sook-Hwan Kim, Jae-Pil Jung
J Weld Join. 2005;23(3):61-67.   Published online July 15, 2005
PDFPDF    
Monitoring and Measurement of Plasma/Plume in Laser Welding Process
Seo-Jeong Park, Sook-Hwan Kim, Young-Gak Kweon
J Weld Join. 2005;23(3):21-25.   Published online July 15, 2005
PDFPDF    
Packaging Technology in Electronics and 3-dimensional Stacking Packaging
Jung-Mo Kim, Jae-Pil Jung, Sook-Hwan Kim, Jai-Hyun Park
J Weld Join. 2005;23(2):23-31.   Published online May 12, 2005
PDFPDF    
Recent Trends in Development of Joining Technologies -Laser Brazing Technology-
Sook-Hwan Kim, Mok-Young Lee, Young-Gak Kweon
J Weld Join. 2004;22(5):13-17.   Published online November 12, 2004
PDFPDF    

Journal of
Welding and
Joining

Print ISSN: 2466-2232
Online ISSN: 2466-2100

Register for e-submission  Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Register for e-submission  Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system.
For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Register for e-submission  Free archive
Anyone may access any past or current articles without logging in.


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2024 by The Korean Welding and Joining Society.

Developed in M2PI